245 | _aCharacterization of axial fracture and delayed hydride cracking behavior of zircaloy cladding tubes | ||
250 | _a | ||
260 | _aMumbai | ||
260 | _bBhabha Atomic Research Centre | ||
260 | _c2011 | ||
300 | _a64 p. | ||
300 | _c29 cm | ||
856 | _u | ||
490 | _aBARC TR E 004 : 2011 | ||
700 | _a | ||
650 | _a | ||
650 | _aReactor safety | ||
650 | _aFuel pins, Reactor cores, Cracking, Stress intensity factors, Fractures, PHWR type reactors, Zircaloy 4 | ||