000 | 00946 a2200301 4500 | ||
---|---|---|---|
001 | 25009 | ||
003 | OSt | ||
005 | 20221210161450.0 | ||
008 | 221210b |||||||| |||| 00| 0 eng d | ||
020 | _a0 | ||
040 | _cIITB | ||
041 | _aeng | ||
080 |
_a043:541.13:620.91 _bSha |
||
100 |
_aSharan, M.K. _eAuthor _931879 |
||
245 | _aPreparation and characterization of a semiconductor material tungsten oxide films for the utilization of solar energy (R) | ||
260 | _aBombay | ||
260 | _bIIT | ||
260 | _c1983 | ||
300 |
_a205 p. _c28 cm |
||
502 |
_aThesis _bPh.D _cIndian Institute of Technology Bombay. Department of Chemistry _d1983 |
||
650 |
_aSharon, M. _931880 |
||
650 |
_aTheses and Dissertations _921 |
||
650 |
_aSolar cells _9385 |
||
650 |
_aSolar energy _9405 |
||
700 |
_aSharon, M. _eSupervisor _931881 |
||
710 |
_aIndian Institute of Technology Bombay _bDepartment of Chemistry _9169 |
||
942 |
_cTD _2udc |
||
999 |
_c163156 _d163156 |